Lead selenide
Technical docking: Gas phase synthesis CVD - a specially designed quartz device, high-precision analysis and weighing, proportioning according to MOL ratio of 1:1, using high-frequency oscillation heating, and cooling circulating water on the quartz device to prevent steam pressure from exploding due to excessive pressure.
1. Physical properties:
Molecular formula: PbSe
Atomic mass: 286.16
Melting point: 1065 ℃
Density: 8.10g/cm3
Physical properties: black powder, with an average particle size of 100 mesh
CAS No.: 12069-00-0
Call the national toll-free hotline for more details
Lead selenide
Technical docking: Gas phase synthesis CVD - a specially designed quartz device, high-precision analysis and weighing, proportioning according to MOL ratio of 1:1, using high-frequency oscillation heating, and cooling circulating water on the quartz device to prevent steam pressure from exploding due to excessive pressure.
1. Physical properties:
Molecular formula: PbSe
Atomic mass: 286.16
Melting point: 1065 ℃
Density: 8.10g/cm3
Physical properties: black powder, with an average particle size of 100 mesh
CAS No.: 12069-00-0
2. Chemical purity: The purity of PbSe is above 99.99%, and the total impurity content of silver, calcium, chromium, copper, iron, magnesium, manganese, nickel, and cobalt is less than 10ppm.
3. Detection method: ICP-MS, ICP-OES
4. Purpose:
Mainly used for infrared detection and manufacturing Photoresistor